INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Rigid Pavements on Expansive Soils

Rigid Pavements on Expansive Soils

Rigid Pavements on Expansive Soils

(OP)
I am working on a project in Fort Worth, Texas. I am looking for some guidence on how to treat the expansive soils for rigid pavement design. The soils are lean clays to fat clays.

PI ranges from 29 to 45
LL ranges from 46 to 62
Percent Swell ranges from 0 to 1.7%
Natural moistures are +/- 1% of the Plastic Limit

The proposed pavement section is 8 r/f concrete over 6 inches of compacted subgrade.

My question is do I need to moisture condition the subgrade soils. If so, to what depth should I over-excavate and moisture condition the soils. Should I lime stabilize the upper 6 to 12 inches of the subgrade? Do I need to put a base material under the concrete pavement? Or can I place the rigid pavement on top of the lime treated subgrade (if I even lime treat the subgrade)

I am looking for some help from professionals that practice in Texas or areas with expansive soils.

Thanks in advance for the reply.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources