Kinematic hardening model
Kinematic hardening model
(OP)
Hi all,
I am not sure why there is a problem with my material model, I seem to be getting an error: "Only one hardening slope is allowed for kinematic hardening".
*Material, name=Co1
*Elastic
230000., 0.3
*Plastic, hardening=KINEMATIC
500., 0.
517., 0.0015
The units are MPa.
I would really appreciate some help, thanks.
I am not sure why there is a problem with my material model, I seem to be getting an error: "Only one hardening slope is allowed for kinematic hardening".
*Material, name=Co1
*Elastic
230000., 0.3
*Plastic, hardening=KINEMATIC
500., 0.
517., 0.0015
The units are MPa.
I would really appreciate some help, thanks.





RE: Kinematic hardening model
Regards
JK7070
RE: Kinematic hardening model
*Material, name=Mat1
*Elastic
231000., 0.3
*Plastic
500., 0.
517., 0.0012
560., 0.02
600., 0.06
650., 0.1
640., 0.1021
This ran well and completed. I just do not understand why the kinematic hardening model gives the error message, "Only one hardening slope is allowed for kinematic hardening"? I would really appreciate some further help.
Thanks.
RE: Kinematic hardening model
517., 0.0015