I am grinding .013"-.015" of hard c
I am grinding .013"-.015" of hard c
(OP)
I am grinding .013"-.015" of hard chrome plating off a spindle that is 33" long and 3.5" dia with a finish of 12 micro @ +/- .001". I have been grinding for almost 10 years. The last 6 grinding on Warner/Swasey, Cincinnati, and Mitsubishi od grinders. Everything i've learned has been on my own, as far as speeds/feeds. The W/S's and Cincinnati's are what I grind these spindles on. I use a "pink" wheel. The best i can do is a 20 min cycle. Is there anything I can do to speed up the machines without damaging the chrome?





RE: I am grinding .013"-.015" of hard c
http://www.georgiagrindingwheel.com/