INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Stress-strain diagram for S235/S275/S355 steel grade.

Stress-strain diagram for S235/S275/S355 steel grade.

Stress-strain diagram for S235/S275/S355 steel grade.

(OP)
Hello,
In my analysis I need to input true stress-strain data in material module. Where can I find, let's say nominal stress-strain data for steel grade S275?

Example data I need:
https://dl.dropbox.com/u/3745405/stress_strain_cur...

RE: Stress-strain diagram for S235/S275/S355 steel grade.

Here is a tip, if you need specific tensile test data have tensile testing performed at nominal cost using actual material. This way, the data is defendable.

RE: Stress-strain diagram for S235/S275/S355 steel grade.

there are several paid services, in our country it is this. look for astm book. or search sciencedirect for data source.

All about materials
http://materialing.com

RE: Stress-strain diagram for S235/S275/S355 steel grade.

(OP)
OK. Thakns.
Does anyone know where can I get Stress-Strain curves for S275 steel according to the Eurocode 3?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources