8620 Steel Carburized
8620 Steel Carburized
(OP)
I received an investment casting, suppose to be 8620 steel, case hardened to 60Rc.
The chemical analysis showed the material to be as follows:
C = .40
Si = .3
Mn = .65
P = .014
S = .010
Cr - .86
Mo - <.01
Ni - .04
Fe = Remainder
Can someone tell me what this material might be?
regards and thanks for your help
JSBC Intl.
The chemical analysis showed the material to be as follows:
C = .40
Si = .3
Mn = .65
P = .014
S = .010
Cr - .86
Mo - <.01
Ni - .04
Fe = Remainder
Can someone tell me what this material might be?
regards and thanks for your help
JSBC Intl.





RE: 8620 Steel Carburized
RE: 8620 Steel Carburized
_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
RE: 8620 Steel Carburized
RE: 8620 Steel Carburized
http://www.metalravne.com/selector/html/aisi.html