INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

mS9490 finishing

mS9490 finishing

mS9490 finishing

(OP)
I've been reading over ms9490 and AMS 5731 and haven't found mention of finishing (passivation, plating, etc) as is called out in specs like NASM 1352. Is there any finishing requirement in MS 9490 that I am not aware of or do these products just come bare?

RE: mS9490 finishing

There is no finishing requirement in MS9490. SAE AMS 5731 specifies the requirements for a corrosion resistant steel, commonly called A286. This grade has inherent resistance to corrosion in ambient atmosphere and other environments. It is usually coated when the mating parts are dissimilar materials.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources