aisi 4340 creep rupture data
aisi 4340 creep rupture data
(OP)
Hi
I'm trying to find some creep rupture data at elevated temperatures for aisi 4340 steel at conditons other than normalized (which I already have). Ideally for material around about a HRC=45.
Any help would be appreciated.
Thanks
allan
I'm trying to find some creep rupture data at elevated temperatures for aisi 4340 steel at conditons other than normalized (which I already have). Ideally for material around about a HRC=45.
Any help would be appreciated.
Thanks
allan





RE: aisi 4340 creep rupture data
RE: aisi 4340 creep rupture data
allan