I recently had some pipe installed for an SO2 line but I made the mistake of having fittings for two different projects sitting next to each other. So when the contractor finished their work I noticed that they had mixed in a few 304Lss fittings with the rest of the project that was 316Lss.
My question is does SO2 corrode 304Lss more than 316Lss?
My question is does SO2 corrode 304Lss more than 316Lss?





RE: Compare Corrosion of 304L to 316Lss with SO2
http://eng-tips.com/viewthread.cfm?qid=324221