INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

SA 312 TP316Ti

SA 312 TP316Ti

SA 312 TP316Ti

(OP)
Are there any tables for Stress Allowance for SA 312 TP316Ti or SA 182 F316Ti? ASME II Part D does'nt cover this material, where can I find Stress Allowance table acceptable to the ASME Code containing this materials. Please reply.

RE: SA 312 TP316Ti

You won't if there are no stress lines in Section II, Part D. You can review if there are Code Cases for this material.

RE: SA 312 TP316Ti

Last time I used this material, the Client and the Third Party Verifier agreed to accept my calculations for allowable stress based on the plate and forgings test results. Not in accordance with the code, but worked for me. I used in preliminary calcs the values for 'H', then I reworked it for the calculated allowables.
Cheers,gr2vessels

RE: SA 312 TP316Ti

(OP)
Thank you guys!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources