PIPE formed in normalising condition A106B
PIPE formed in normalising condition A106B
(OP)
We are using 26" pipe as shell for H2S stripper vessel. The design requires A106B normalised Pipe. We can only get pipe formed in Normalised condition. Can we use the pipe.





RE: PIPE formed in normalising condition A106B