Air set casting sand
Air set casting sand
(OP)
Can anyone point me to a supplier for said sand and binder systems for use with Al alloy.
Supplier must be in the Uk, and be willing to ship a min quantity of 1/2 - 1 ton + same ratio of binder to Ireland.
Thanks in advance,
Brian,
Supplier must be in the Uk, and be willing to ship a min quantity of 1/2 - 1 ton + same ratio of binder to Ireland.
Thanks in advance,
Brian,






RE: Air set casting sand
RE: Air set casting sand
Max Quantity same - 1/2 - 1 ton.
I found a place late lastnight after a lot of looking, emailed them, and looks promising,
http://www.johnwinter.co.uk/foundry-products/sand-binders
Brian,
RE: Air set casting sand
Foseco, Ashland Chemicals, must be able to help you I suppose.