Smart questions
Smart answers
Smart people
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Member Login

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips now!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

Join Eng-Tips
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

LINK TO THIS FORUM!

Add Stickiness To Your Site By Linking To This Professionally Managed Technical Forum.
Just copy and paste the
code below into your site.

Partner With Us!

"Best Of Breed" Forums Add Stickiness To Your Site
Partner Button
(Download This Button Today!)

Feedback

"Because of this forum, I continue to WOW! my clients!"

Geography

Where in the world do Eng-Tips members come from?

Strain in fiberglass wing panel in various temperatures

KtAero (Aerospace)
9 May 12 13:01
I have several full bridge bending bridges set up on a fiberglass airplane wing to measure wing bending along the span. Should be thermal compensated with full bridge, but I'm getting significant (equivalent to hundreds of in-lb) thermal impact (roll from hanger into sun and trace drifts, or cloudy day drifts for about 15 min following takeoff as wing finds cooler equilibrium). I think this is mechanical- that the wing is actually physically straining, but I need a way to subtract off the drift and would like to do it automatically. I can do this by 1) waiting for temps to equalize 2) look only at short time (several seconds) where the drift is insignificant. However, this doens't allow me to correlate a known wing load in the hanger to a particular wing strain that can be used to determine strains in flight since the temp changes the strain/load relationship. Ideas? Thanks

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!

Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close