Concerned to Welder Performment
Concerned to Welder Performment
(OP)
Dear all,
I have a problem about welder.
when i qualify welder so do i need third party for witnessing and suppply certificate?
my think, there are constructor and client is enough.
I have a problem about welder.
when i qualify welder so do i need third party for witnessing and suppply certificate?
my think, there are constructor and client is enough.





RE: Concerned to Welder Performment
Are you the Contractor's company inspector testing your own welders?
RE: Concerned to Welder Performment
RE: Concerned to Welder Performment
RE: Concerned to Welder Performment
RE: Concerned to Welder Performment
As per BSEN 287-1 - TPI Witnessing & Certification for Welder Qualification is required.
Summary
Witnessing & Certification of Welder Qualification depends upon the Standards used. Apart from that it depends upon the Client's requirement/Project Requirement.
RE: Concerned to Welder Performment
My recommendation is to seek the services of an individual certified to AWS QC1 as a Senior Certified Welding Inspector and if you cannot find one then seek someone that is qualified to AWS QC1 as a Certified Welding Inspector.
Best regards - Al