Smart questions
Smart answers
Smart people
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Member Login

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips now!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

Join Eng-Tips
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

LINK TO THIS FORUM!

Add Stickiness To Your Site By Linking To This Professionally Managed Technical Forum.
Just copy and paste the
code below into your site.

Partner With Us!

"Best Of Breed" Forums Add Stickiness To Your Site
Partner Button
(Download This Button Today!)

Feedback

"...These forums are an excellent source and example of the way people can help each other..."

Geography

Where in the world do Eng-Tips members come from?
ISDQAQC (Specifier/Regulator)
2 May 12 15:18
Looking over an engineering report, three components to a vessel are given a MDMT of 2. all other components are -20. The CET value is shown as -47 and the equipment MDMT is 2.

the 3 three components are, a bottom shell ring, 30" O.D. nozzle and the repad for the nozzle. all are 1.1250 and SA-516-Gr. 70. The resolution is for a brittle fracture assessment in accordance with API 579-1. I would welcome all assistance. thank you..   
SJones (Petroleum)
3 May 12 3:40
What are the MAT values?

Steve Jones
Materials & Corrosion Engineer

http://www.linkedin.com/pub/8/83b/b04
 

metengr (Materials)
3 May 12 7:52
In addition to MAT, which can be the minimum design metal temperature using ASME Section VIII, Div 1 design basis, what exactly are you trying to do under API/ASME FFS-1 brittle fracture assessment? Are you trying to re-rate this vessel?
LSThill (Mechanical)
3 May 12 11:56
ISDQAQC (Specifier/Regulator)

HAVE YOU REVIEW THE FOLOWING:


API 579-2/ASME FFS-2 2009 Fitness-For-Service Example Problem Manual
ASSESSMENT OF EXISTING EQUIPMENT FOR BRITTLE FRACTURE EXAMPLE PROBLEMS
page 3-1 3-21
3.1 Example Problem 1 ......................................................................................................... 3-1
3.2 Example Problem 2 ......................................................................................................... 3-1
3.3 Example Problem 3 ......................................................................................................... 3-1
3.4 Example Problem 4 ......................................................................................................... 3-2
3.5 Example Problem 5 ......................................................................................................... 3-3
3.6 Example Problem 6 ......................................................................................................... 3-4
3.7 Example Problem 7 ......................................................................................................... 3-6
3.8 Example Problem 8 ......................................................................................................... 3-8
3.9 Example Problem 9 ....................................................................................................... 3-10
3.10 Example Problem 10 ..................................................................................................... 3-11
  

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!

Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close