Flakes Of steel coming our of CS SMLS Pipes
Flakes Of steel coming our of CS SMLS Pipes
(OP)
Hello experts,
On our recent supplies of CS SMLS API5L B Pipes for a project in UAE, our clients have reported a problem. upon witnessing, flakes of steel are coming out when the pipes are shot blasted for paintings.
please advise what can be the cause of such problem
On our recent supplies of CS SMLS API5L B Pipes for a project in UAE, our clients have reported a problem. upon witnessing, flakes of steel are coming out when the pipes are shot blasted for paintings.
please advise what can be the cause of such problem





RE: Flakes Of steel coming our of CS SMLS Pipes
RE: Flakes Of steel coming our of CS SMLS Pipes
Is it metal or actually just scale flaking off?
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
RE: Flakes Of steel coming our of CS SMLS Pipes
RE: Flakes Of steel coming our of CS SMLS Pipes
RE: Flakes Of steel coming our of CS SMLS Pipes
RE: Flakes Of steel coming our of CS SMLS Pipes
rp