INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

3.1645 AlCuMgPb Material?

3.1645 AlCuMgPb Material?

3.1645 AlCuMgPb Material?

(OP)
Hello,

I have a drawing from Germany with this material called out "3.1645 AlCuMgPb".  I am wondering what this would be comprable to? The International Registration Record (AA) U.S.A. Specs calls this a "2007" material?  Any help would be appreciated.

RE: 3.1645 AlCuMgPb Material?

It's a 2000 series aluminum alloy with the following chemical composition limits in weight percent:

Cu 3.3 - 4.6
Fe 0.8 Max
Mg 0.4 - 1.8
Mn 0.10 Max
Si 0.8 Max
Ti 0.20 Max
Zn 0.8 Max

Balance is aluminum.

Maui

www.EngineeringMetallurgy.com

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources