Leeb Temperature correction for steel
Leeb Temperature correction for steel
(OP)
I'm working on some hardness testing and it's over the ASTM A956-06 temp requirement for the Leeb hardness test. the test is valid for 40 deg. F to 100 deg. F. and I'm testing at 200 deg. F. the standard says to develop a temperature correction for the material being tested. I've searched everywhere and cannot get a hint on how to go about this. My material is A516 grade 70 steel. If anyone has any ideas I would appreciate it thanks.