Smart questions
Smart answers
Smart people
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Member Login

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips now!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

Join Eng-Tips
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

LINK TO THIS FORUM!

Add Stickiness To Your Site By Linking To This Professionally Managed Technical Forum.
Just copy and paste the
code below into your site.

Partner With Us!

"Best Of Breed" Forums Add Stickiness To Your Site
Partner Button
(Download This Button Today!)

Feedback

"...you guys have given us a way of asking a question and getting some very timely feedback from other users so we don't have to re-invent the wheel time and again..."

Geography

Where in the world do Eng-Tips members come from?
Toxotoxo (Industrial)
31 Mar 12 19:09
Does anyone know what type of rubber is used in this product http://www.josephjoseph.com/kitchen-tools/elevate .


Also what is the manufacturing process called in which a plastic is coated in rubber?

thanks in advance
Metten (Materials)
2 Apr 12 1:56
I personally doubt it is rubber. The carousel set has a base in rubber, are you sure the utensils do too?
btrueblood (Mechanical)
2 Apr 12 10:22
Mfg. process = overmolding.

Rubber possibilities might be santoprene, or other injection-moldable (thermally processed) elastomers, these are the most commonly used.  It would be possible to overmold with just about any rubber, provided the handle material can survive the 250-350 deg. F rubber curing temperature for 1/2 hour or so.  Generally, the slower processing time of cured rubber makes it more expensive than the melt-processable elastomers.
GrahamBennett (Materials)
6 Apr 12 11:10
The handles are probably a grade of TPE such as Santoprene.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!

Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close