INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Welder testing

Welder testing

Welder testing

(OP)
Can anyone advise on following?
When testing welder to AWS D1.1 is the material an essential variable. As you are testing the welder skill to use consumable & not material.
 

RE: Welder testing

D1.1 is only applicable to carbon steel and high strength low alloy steel. Qualification using any of the steels listed in Table 3.1 qualifies the welder for any steel listed in D1.1.

Best regards - Al  

RE: Welder testing

Eck, you can see Table 4.12 for essential available whatever you need to care.  

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources