Weld Overlay Cladding
Weld Overlay Cladding
(OP)
We have to make weld overlay cladding of SS304 on carbon steel.
What we normally do is, first buttering with ER309 then we wuse ER308.
I come to know that there is a SS wire that is directly used on CS without buttering. It has properties of both ER309 and ER308.
Does anybody know, the name of this wire? its manufacturer?
What we normally do is, first buttering with ER309 then we wuse ER308.
I come to know that there is a SS wire that is directly used on CS without buttering. It has properties of both ER309 and ER308.
Does anybody know, the name of this wire? its manufacturer?
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED