Chrysler Welding Bolts - Projection Welding Standard ?
Chrysler Welding Bolts - Projection Welding Standard ?
(OP)
Greetings, I have Chrysler Process Standard for welding nuts but not for welding bolts.
I have 2 stampings (1.5mm thick) that I am welding a M6x1 weld bolt in. Need guidance on push-off capabilities.
Thanks,
richards49323
I have 2 stampings (1.5mm thick) that I am welding a M6x1 weld bolt in. Need guidance on push-off capabilities.
Thanks,
richards49323





RE: Chrysler Welding Bolts - Projection Welding Standard ?
RE: Chrysler Welding Bolts - Projection Welding Standard ?
I cant seem to locate it.
Thanks again,
richards49323
RE: Chrysler Welding Bolts - Projection Welding Standard ?
https://essd.extra.chrysler.com/ESSD/Login.jsp