INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

DLN 360-200, Diamond-like Nanocomposite coating

DLN 360-200, Diamond-like Nanocomposite coating

DLN 360-200, Diamond-like Nanocomposite coating

(OP)
Hi All,

I'm looking for a supplier able to coat DLN 360-200, Diamond-like Nanocomposite coating (a process Dylyn (R) from Bekaert Advance Coating). Location is not an issue, UPS or DHL can solve the problem. Attached with the detail spec for your reference. Do let me know your contact for such coating service.

Many thanks,
J.J.

RE: DLN 360-200, Diamond-like Nanocomposite coating

JJ,

The Dylyn technology is now part of Sulzer Metco.  They have locations in Europe, USA, and China that perform coating, in addition to selling equipment.  Here is a link with contact information:

http://thinfilm.sulzermetco.com/l_ueber_uns_gb.html
 

RE: DLN 360-200, Diamond-like Nanocomposite coating

(OP)
Hi TYP, appreciated the info...J.J.

RE: DLN 360-200, Diamond-like Nanocomposite coating

(OP)
Hi TVP, sorry for the wrong name in my early respond...J.J.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources