How long after after grouting an auger cast pile can that pile be tested? Is there a minimum time or is it only based on the tested grout strength?
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Auger cast pile testing
I had a contractor test after three days when the grout cube breaks were low.
The pile failed the test and they had to sink another one.
It cost them about a week and a half to remobilize and wait 7 days as they were advised to do in the first place.