I am looking for a material to create butterfly clamps (a.k.a. spring clips) that must withstand 1000 degrees Fahrenheit. Anyone have any suggestions?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
High Temp. Spring Materials
|
RE: High Temp. Spring Materials
If cost is more important try 316 stainless.