INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Levels of sulfate and chloride in soil vs concrete attachk

Levels of sulfate and chloride in soil vs concrete attachk

Levels of sulfate and chloride in soil vs concrete attachk

(OP)
Trying to find any references or standards regarding levels of sulfate or chloride in soil that may cause attack to foundation concrete.  Any guideline tables indicating potential attach levels?

RE: Levels of sulfate and chloride in soil vs concrete attachk

Chlorides external to the concrete will have a negligible effect on the concrete.  Internal chlorides are to be avoided.

Sulfate attack from soils can be detrimental to the concrete.  See ACI 201.2, particularly Table 2.3 for sulfate limits.

 

RE: Levels of sulfate and chloride in soil vs concrete attachk

Lee Daniels, Virginia Tech has information on sulfate in soil.  Mostly related to the mining business and those areas where grass won't grow (i.e., where the oxidation of sulfides leads to sulfuric acid and difficulties with vegetation of construction sites.

Not much of a chemist myself though. . .

f-d

¡papá gordo ain't no madre flaca!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources