INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASTM A-540 Supplementary Requirements S2. Macroetch Test

ASTM A-540 Supplementary Requirements S2. Macroetch Test

ASTM A-540 Supplementary Requirements S2. Macroetch Test

(OP)
This Supplementary Requirement foot note states that the quality and cleanliness may be specified by the purchaser as equal to or better than that indicated by a designated letter and plate number of Military Standard—430 (latest revision).
I've conducted a google/bing search and cannot locate this Military Standard—430.
Any help would be appreciated.

Thanks in advance for your time.

RE: ASTM A-540 Supplementary Requirements S2. Macroetch Test

QAFitz;
Supplement 2 of ASTM A 540 refers you to ASTM E380 Macroetch Testing, Inspection, and Rating Steel Products, Comprising Bars, Billets, Blooms, and Forging. I reviewed an earlier edition of this specification and they have pates for rating. There is a footnote in this specification where you can purchase the referenced plates for rating directly from ASTM.
 

RE: ASTM A-540 Supplementary Requirements S2. Macroetch Test

Sorry for the typo, the above should be ASTM E 381, not E 380.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources