INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Table PW-39.1

Table PW-39.1

Table PW-39.1

(OP)
I have a question regarding Table PW-39.1 of ASME Section I.

Is interpolation permitted when using Table PW-39.1? It is nowhere mentioned in Section I as I know.

Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN

RE: Table PW-39.1

No, the values in this table cannot simply be interpolated like the  relationship between temperature and allowable stress values. Table 39.1 is a time/temperature relationship derived from a parametric equation, similar to the Larson-Miller creep equation. For interpolation you would need to know the actual equation and constant to determine a time,  based on a known PWHT.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources