Joint configuration is an essential variable as per QW-288 in Section IX.
Can Groove plus fillet weld procedure be applied to fillet weld only production joint provided all other essential variables are not changed?
QW-288 does not talk about fillet welds, it only addresses groove joint.
Can Groove plus fillet weld procedure be applied to fillet weld only production joint provided all other essential variables are not changed?
QW-288 does not talk about fillet welds, it only addresses groove joint.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN





RE: QW-288
Look at QW-288 1 (b) change in groove type and the addition or deletion of prelaced weld metal. You have a production joint where a fillet weld is required, in lieu of a partial penetration tube to tubesheet groove weld. To me, this is a change in weld joint configuration, and is an essential variable change - meaning re-qualification.