Gasket Oversized
Gasket Oversized
(OP)
Hi Gents,
I'd like to know what can happen if I install a oversized gasket (AISI 316) between body and bonnet of a gate valve (F6NM). Any consideration will be appreciated
Wreg
I'd like to know what can happen if I install a oversized gasket (AISI 316) between body and bonnet of a gate valve (F6NM). Any consideration will be appreciated
Wreg





RE: Gasket Oversized
If its a different diameter it probably won't seal.
If its a different height it may not drift, unless its reverse acting, in which case the vbsm may not seal.
RE: Gasket Oversized
RE: Gasket Oversized