Sand Cast Steel foundry that can pour 13k pounds?
Sand Cast Steel foundry that can pour 13k pounds?
(OP)
Hi All, I'm working a two large motor housing designs that weigh about 13k pounds. Do you know of any foundries that can manufacture this in one piece? I'm having trouble finding foundries in the US that can do cast steel in this weight.
thanks,
nick
thanks,
nick





RE: Sand Cast Steel foundry that can pour 13k pounds?
_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
RE: Sand Cast Steel foundry that can pour 13k pounds?
RE: Sand Cast Steel foundry that can pour 13k pounds?
arun, thanks i'll keep that in mind.
RE: Sand Cast Steel foundry that can pour 13k pounds?
weldment?
Here are few more possible sources.
Contact the Texas Branch
http://www.cabinc.com/index.html
http://www.columbiasteel.com/custom-castings.html
RE: Sand Cast Steel foundry that can pour 13k pounds?
RE: Sand Cast Steel foundry that can pour 13k pounds?
RE: Sand Cast Steel foundry that can pour 13k pounds?
There are still a few large foundries in the UK. Sheffield Forgemasters has a good reputation for quality, and I'm pretty sure that size is within their capability. Not really my field of expertise but they did a fair bit of complex work for a previous employer. ht
----------------------------------
If we learn from our mistakes I'm getting a great education!
RE: Sand Cast Steel foundry that can pour 13k pounds?
ht
We have used a few of the one that came up on the quick search I just did.
BARBERTON STEEL INDUSTRIES Barberton OH U.S.A.
COLUMBIANA FOUNDRY CO Columbiana OH
MAYNARD STEEL CASTING CO Milwaukee WI U.S.A.
We have delt with.
FALK - REXNORD LLC Milwaukee WI U.S.A.
We have not delt with them but I have hear are impressive.
We use Southland for importing alot of our castings and I know they make Baldors castings.
I can not say enough about making sure you have very good pattern and core boxes.
Bradken - Amite did some good work for us years ago and did a lot of post casting machining and painting too.