INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

K mold testing

K mold testing

K mold testing

(OP)
Does anyone know what I can use to coat a k mold. In the past I used a certain type of graphite, it worked great but I don't know where to get it. Currently I am using a dry graphite from a spray can, this not working too well. The mold is getting too hot and my samples have heat shrinkage.

RE: K mold testing

Hi. The coating doesnt cool the mold. Before i need to know if you only want to look for oxides on aluminum alloy or need asny further data. If just looking for oxides you need to wait some time before pour the next specimen. The graphite as coat is working well, also can coat with permcoat. Hope this result helpful for you.  

RE: K mold testing

(OP)
Thanks for your response. I will look for permcoat. In the past I could pour 20 samples, no problem. Now I can only pour 10 or 12 and my mold is too hot, using the graphite spray. I wonder is there some type of ladle coating I can use?

Jerry Davis, 25 years experience in aluminum die casting

RE: K mold testing

(OP)
Yes I am looking for oxides in A383 aluminum alloy.

Jerry Davis, 25 years experience in aluminum die casting

RE: K mold testing

RE: K mold testing

(OP)
OK, Thank you. I wiil look there.

Jerry Davis, 25 years experience in aluminum die casting

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources