INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AWS D1.1 Table 4.5 # 13- Process Parametres

AWS D1.1 Table 4.5 # 13- Process Parametres

AWS D1.1 Table 4.5 # 13- Process Parametres

(OP)
Dear Experts
Onsite AC & DC current used- Root using LB52U x AC for better penetration- 1 WPS(AC) & Fill/Cap- using LB52 x DC using another WPS(DC).Weld Process-SMAW
So 2 diffrernt WPS with varying AC/DC Variables used for welding this T-K-Y Joints.
Based on  Table 4.5 # 13- straightway it is non-conformance but
In this combination case is it really violating the code requirements?
No new WPS written combining the 2 PQRs.

100% UT/MT completed.
Pls be patient and appreciate open-minded response asap

RE: AWS D1.1 Table 4.5 # 13- Process Parametres

If you are using AWS D1.1-2011, refer to clause 3.6.1.

Best regards - Al  

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources