Welding to 1 3/4" Thick Flange
(OP)
Hi guys, have a project where will be welding to flange of existing W 12x190 column. Has a flange thickness of 1 3/4". Will that welding require preheat?
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Welding to 1 3/4" Thick Flange
|
RE: Welding to 1 3/4" Thick Flange
See AWS D1.1. Chapter 3
Before you get started, you need to ask: What grade of steel? If you don't know, assume the worst (higher grade / category).
RE: Welding to 1 3/4" Thick Flange
[b]a hundred-and-a-half at an inch-and-a-half[/b]
RE: Welding to 1 3/4" Thick Flange
RE: Welding to 1 3/4" Thick Flange
RE: Welding to 1 3/4" Thick Flange