AISI 5115 Bar Supplier
AISI 5115 Bar Supplier
(OP)
I am attempting to locate a domestic supplier in the United States for 3 inch to 5 inch diameter round bars of AISI 5115 (DIN 1.7131 or 16MnCr5). Does anyone have any suggestions regarding companies or distributors who are likely to carry this product? A typical chemical composition for this grade in weight % is: 0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.99% Cr, 0.02% Mo, 0.12% Ni, 0.010% V, 0.015% Al.
Maui
Maui





RE: AISI 5115 Bar Supplier
Gerdau Macsteel produces this grade, but I am not sure if they have it stocked in "distributor" quantities:
http://ww
Eaton Steel & Turret Steel both show 5120 as part of their inventory/stock list, so you may want to compare their spec against yours:
http://www.eatonsteel.com/esbchome.nsf/inventory
htt
RE: AISI 5115 Bar Supplier
I am sure both steel mills have 5115 in billet/bloom form.