INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Welding Procedure Specification for review

Welding Procedure Specification for review

Welding Procedure Specification for review

(OP)
Hello everyone, here are the variables and information about the WPS, let me know what you think: 4130 to the same.

1. Base metals: ASTM A-510-06 GRADE 4130 to the same
2. Purpose: For welding the last API flanges on a wellhead
3. filler metals: GTAW (ER80SNi-1)root and hot pass, then Flux Core (E71T-12M) fill and cap
4. Pre-heat: 300 F minimum
5. PWHT: 1250+-25F 1hr/inch of thickness, but not less than 1.5hr
6. Base metal thickness: 0.600"
7. Thickness range qualified: 0.1875" - 1.200"
8. Charpy Impact testing: None (No temperature; service or ambient is anticipated to get below -20F)
9. Position and progression: All and Upwards
10. Additional question: At what temperature and/or thickness do I worry about Charpy Impact testing for this procedures.

Thank you very much for your help!  
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources