I'm looking for a recommendation for a threaded insert to be used in Acetal, with #6 stainless steel hardware. Will be cycled about a dozen times a day.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Threaded inserts for plastic
|
RE: Threaded inserts for plastic
SI® Ultrasonic / Heat Staking Inserts
http:
Dodge® inserts
http://www
Fastening with metal screws (Ticona)
http:/