INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME VIII UCS 66 Curves

ASME VIII UCS 66 Curves

ASME VIII UCS 66 Curves

(OP)
Does anybody know how I can EXTRAPOLATE Fig UCS-66 Curves upto 250mm thickness

RE: ASME VIII UCS 66 Curves

Extrapolation not necessary; final thickness notation at bottom of chart is >/= 75mm.  Because it flatlines at 75mm, use that value as appropriate for your intended material/thickness..

RE: ASME VIII UCS 66 Curves

Elise, perhaps you had better read UCS-66.

Odd question for the forum.

Regards,

Mike

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources