Cellulose acetate
Cellulose acetate
(OP)
Can I Mix CA with DOP and product some parts with it?
(I have experience for producing of PVC ,PVC-E+DOP ,in my home, in my wife's oven)
Is there any online information about formulation and process?
Thanks
(I have experience for producing of PVC ,PVC-E+DOP ,in my home, in my wife's oven)
Is there any online information about formulation and process?
Thanks