INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

MAOP

MAOP

(OP)
I'll been asked to calculate the MAOP of our pipelines and risers. my concern is some line have a combination of flexible hose and carbon steel pipe. I can give the lowest MAOP base on the hose rating  base on the design pressure.I have gather some UT inspection of wall thickness of the pipe and some of them are 30 years of age I have given 3mm corrosion allowance for is it the right thing to calculate

RE: MAOP

The MAOP for the flexible might not be the MAOP for the steel pipeline.  In no way can you ascribe a 3 mm corrosion allowance without detailed knowledge of the current integrity status of the system.  Try a Google search on: pipeline integrity, pipeline fitness for service; pipeline rerating

Steve Jones
Materials & Corrosion Engineer

http://www.linkedin.com/pub/8/83b/b04
 

RE: MAOP

"Corrosion allowance" is something you assign at the beginning of life (or at the time of re-rating) to determine an effective life of the pipe.  So, if you are designing a pipeline using 0.322 inch wt 8-inch nominal pipe, you have to subtract your corrosion allowance from the actual wall thickness to determine the metal mass that participates in the strength calculation.

You pick that corrosion allowance based on expected wastage per year times the number of years you are planning for the pipe to last.  Let's say that the expected life was 30 years and the corrosion allowance was 3 mm.  That says that your current pipe wall thickness should be assumed to be 3 mm thinner than original (i.e., the corrosion allowance is gone).  

Now if you are re-rating the pipe for another 30 years, you can either measure the current wall thickness in a large number of places (take readings all around the pipe at every place you anticipate higher-than-normal corrosion rates) and then use the minimum value measured (not the average) as your new wall thickness.  Subtract the corrosion allowance from that and calculate the new MAWP based on the remaining metal mass.

David

RE: MAOP

(OP)
thank you guys for all the feed back it really helps a lot

RE: MAOP

(OP)
David

That Exactly what details I got now.. what I need is a formula calculation..

RE: MAOP

For gas look at ASME B31.8.

David

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources