Design properties of Coniferous species C24
Design properties of Coniferous species C24
(OP)
Does anyone have information on the structural design properties of Coniferous Species C24. Thanks
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Design properties of Coniferous species C24
|
RE: Design properties of Coniferous species C24
RE: Design properties of Coniferous species C24
RE: Design properties of Coniferous species C24
http
RE: Design properties of Coniferous species C24
RE: Design properties of Coniferous species C24
it is important to note that it may be a bit more complicated than comparing the design stresses. There are probably different testing regimes and probability of exceedence e.t.c.
What is the reason you need this information?
RE: Design properties of Coniferous species C24
RE: Design properties of Coniferous species C24
i.e:
wet timber has a lower permissible stress than dry.
long-term loads have a lower permissible stress than short-term etc.
RE: Design properties of Coniferous species C24
"Mechanics of wood and wood composites"..
there are some tables that tabulated the issue.
hope that helps
Milad Mohamadzadeh
Wood Structural Engineer
RE: Design properties of Coniferous species C24
Which country is this timber structure in and what codes are you using?
RE: Design properties of Coniferous species C24