Hardenability of L-80 13 Cr material as per API 5CT
Hardenability of L-80 13 Cr material as per API 5CT
(OP)
Please can somebody tell me about hardenability requirement as per API 5CT for Coupling 3-1/2" L-80 13Cr material.
We have received hardness report after tempering, but hardenabilty hardness values for as quenched condition are not mentioned in MTC. As per my interpretation with code, hardenabilty test to be carried out.(Reference API 5CT, clause 7.10.2)
We have raised discrepancy about this and conveyed to manufactuer.
But manufacturer clarifies that hardeneability requirement is not mandatory.
We have received hardness report after tempering, but hardenabilty hardness values for as quenched condition are not mentioned in MTC. As per my interpretation with code, hardenabilty test to be carried out.(Reference API 5CT, clause 7.10.2)
We have raised discrepancy about this and conveyed to manufactuer.
But manufacturer clarifies that hardeneability requirement is not mandatory.





RE: Hardenability of L-80 13 Cr material as per API 5CT