INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

neoprene pads at expansion joints

neoprene pads at expansion joints

neoprene pads at expansion joints

(OP)
What type of neoprene specifically would you recommend for bearing pads at expansion joints?

What value on the Durometer chart?

Please see the link for the specifics.

Specifically for WF girder bearing and roof joist bearing..

RE: neoprene pads at expansion joints

A2...Neoprene, Shore A=70  

RE: neoprene pads at expansion joints

(OP)
You're the man Ron, hoping you'd answer my RFI for me :)

RE: neoprene pads at expansion joints

(OP)
They also used the same term "Shore" in their example, what does that mean? Some guy named Shore who came up with this scale?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources