INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Steam NH3 threshold for Brass SCC?

Steam NH3 threshold for Brass SCC?

Steam NH3 threshold for Brass SCC?

(OP)
I understand that it primarily occurs at pH>8.5, but is there a general ammonia content threshold below which season cracking is unlikely to occur in steam service? Thanks in advance.

RE: Steam NH3 threshold for Brass SCC?

I would be more concerned with ammonia grooving than SCC in steam service. Example - brass condenser tubes which are exposed to wet steam conditions on the OD and cooling water on the ID surface.

RE: Steam NH3 threshold for Brass SCC?

I think it is usually a dangerous game to rely on temperature, pH, concentrations, etc, to prevent SCC; there is always an upset. That being said our refineries would use Admiralty in streams with H2S, it was some protection.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources