Alumina Alternative
Alumina Alternative
(OP)
Hello,
I am currently looking for a material that has similar properties to Alumina.
In the past we've looked at alternatives Albemet 162, 6061 Aluminum, 303 SST, AlSic, Titantium, 99% Alumina, Moly alloys, and T-Con.
Looking at something that has high stiffness, stronger than, or as strong as, Aluminum, preferably on the cheap side and can retain properties in environments around 1000°C.
We're open to any type of materials including fiberglass, ceramics and metals.
Thank you
I am currently looking for a material that has similar properties to Alumina.
In the past we've looked at alternatives Albemet 162, 6061 Aluminum, 303 SST, AlSic, Titantium, 99% Alumina, Moly alloys, and T-Con.
Looking at something that has high stiffness, stronger than, or as strong as, Aluminum, preferably on the cheap side and can retain properties in environments around 1000°C.
We're open to any type of materials including fiberglass, ceramics and metals.
Thank you





RE: Alumina Alternative
Bruce
www.accuratus.com
RE: Alumina Alternative
RE: Alumina Alternative
Comprehension is not understanding. Understanding is not wisdom. And it is wisdom that gives us the ability to apply what we know, to our real world situations
RE: Alumina Alternative
Any suggestions would be most welcome.