Can anyone answer me to the following question?
I have to make a data sheet for the Titanium 6.2.4.6 (UNS R56260) and I need to put the following information:
- tipical Yeld/Tensile ratio. (0.8 - 0.93 my proposal)
- Minimum acceptable Charpy V-Notch (-46C).(>=15J my proposal)
Could be right my proposal?
Thanks in advance to anyone may help me.
I have to make a data sheet for the Titanium 6.2.4.6 (UNS R56260) and I need to put the following information:
- tipical Yeld/Tensile ratio. (0.8 - 0.93 my proposal)
- Minimum acceptable Charpy V-Notch (-46C).(>=15J my proposal)
Could be right my proposal?
Thanks in advance to anyone may help me.





RE: TITANIUM 6.2.4.6 (UNS R56260)
http://www.timet.com/6-2-4-6frame.html
Use the reference below for additional information
h