INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

FRACTURE TOUGHNESS TESTING EXEMPTIONS PER PARA 841.1.2(a), B31.8 2010

FRACTURE TOUGHNESS TESTING EXEMPTIONS PER PARA 841.1.2(a), B31.8 2010

FRACTURE TOUGHNESS TESTING EXEMPTIONS PER PARA 841.1.2(a), B31.8 2010

(OP)
Para 841.1.2(a) OF ASME 31.8 2010 provides stress level guidelines below which fracture toughness criterion or other method need not be applied. However, succeeding paragraphs (b) Brittle Fracture Control testing and (c) Ductile Fracture Arrest testing seem to be required.  Furthermore, Interpretation 15-5 states these tests are required.  Do paragraphs 841.1.2(b) and (c) and Interpretation 15-5 over ride the testing exemption provided in 841.1.2(a)?  Please help. Thanks.
JRCarmen
 

RE: FRACTURE TOUGHNESS TESTING EXEMPTIONS PER PARA 841.1.2(a), B31.8 2010

Interpretation 15-5 pertains to testing to verify the fracture toughness criterion, i.e. when the exemption criteria have not been met.  The exemption criteria are for brittle and ductile fracture; therefore, if they are not met then testing for brittle and/or ductile fracture control are required.

Steve Jones
Materials & Corrosion Engineer

http://www.linkedin.com/pub/8/83b/b04
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources