INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

MPI on AISI 410

MPI on AISI 410

MPI on AISI 410

(OP)
I have received NDE Report (Magnetic Particle Inspection) for wellhead material AISI 410. As per my knowledge AISI 410 is martensitic stainless steel having paramagnetic properties. Please let know wheather 410 is paramagnetic or ferromagnetic and applicability of MPI on it.

Regards

RE: MPI on AISI 410

Hi gafoorkti

Look at this :

" Martensitic and Precipitation Hardenable Stainless Steels

All Martensitic and most precipitation Hardenable stainless steels are ferromagnetic.  Due to the stresses induced by the hardening transformation, these grades exhibit permanent magnetic properties if magnetized in the hardened condition.  For a given grade, the coercive force, Hc, tends to increase with increasing hardening, rendering these alloys more difficult to demagnetize.

Examples of martensitic stainless steels are Type 410, 416, 420, 440B and 17-4. "

Source : Magnetic Behavior of Stainless Steels
http://www.mceproducts.com/knowledge-base/article/article-dtl.asp?id=18

RE: MPI on AISI 410

MPI is a very suitable surface nondestructive test (NDT) for martensitic stainless steels, like 403 or 410.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.