P355GH IN SECTION VIII-1
P355GH IN SECTION VIII-1
(OP)
In 2010 Edition of Section VIII-1, P-355GH is added in table UCS-23 but its allowable stress values are not included in Table 1A of Section II Part D as opposed to other EN materials that ASME has permitted like P295GH etc.
In order to take its allowable stress, Appendix 1 of Section II Part D shall be followed. Without knowing UTS values at elevated temperatures, allowable stress value can not be computed from Appendix 1 of II-D.
EN 10028 provides only yield strength values of P355GH at elevated temperatures but not UTS, so any help from where I can obtain its UTS values at elevated temperature?
In order to take its allowable stress, Appendix 1 of Section II Part D shall be followed. Without knowing UTS values at elevated temperatures, allowable stress value can not be computed from Appendix 1 of II-D.
EN 10028 provides only yield strength values of P355GH at elevated temperatures but not UTS, so any help from where I can obtain its UTS values at elevated temperature?
Nasir