Welding of different grades
Welding of different grades
(OP)
Hi all,
Can we weld a 483 grade line with a 359 grade flange without problems providing that the filler metal will be of higher grade of course?
Thanks for the help
Can we weld a 483 grade line with a 359 grade flange without problems providing that the filler metal will be of higher grade of course?
Thanks for the help





RE: Welding of different grades
TheWeldingHandbook
www.docstoc.com › Technology ›
RE: Welding of different grades
Why do you believe that the welding filler metal needs to match the higher strength grade?