INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

API-934

API-934

(OP)
Hi ,

Can anyone tell me why do we use API-934, is it an additional requirement for 2 1/4Cr-1 Mo & 3Cr- 1Mo materials.
Can it be waived off..?

Thanks,

RE: API-934

Khati,

When I googled "API 934" I found the following excerpt from IHS (which is a service that provides access to standards):

"This recommended practice presents materials and fabrication requirements for new 2-¼Cr and 3Cr steel heavy wall pressure vessels for high temperature, high pressure hydrogen service. It applies to vessels that are designed, fabricated, certified and documented in accordance with ASME Code Section VIII, Division 2, including Appendix 26, Mandatory Rules for Cr-Mo Steels with Additional Requirements for Welding and Heat Treatment and ASME Code Case 2151, as applicable.

Materials covered by this recommended practice are conventional steels including standard 2-¼Cr-1Mo and standard 3Cr-1Mo steels, and advanced steels including enhanced 2-¼Cr-1Mo, 2-¼Cr-1Mo-¼V, 3Cr-1Mo-¼V-Ti-B, and 3Cr-1Mo-¼V-Cb-Ca steels. The interior surfaces of these heavy wall pressure vessels may have an austenitic stainless steel weld overlay to provide additional corrosion resistance."

In regard to your question about whether the standard can be waived off -- it would seem to me that would be between you and your customer.
 

Patricia Lougheed

******

Please see FAQ731-376: Eng-Tips.com Forum Policies: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources